Polymer Property : Melt Flow = 0.050 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
SABIC F00952 High Density Polyethylene for Blown Film
Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
SABIC F00952EQ High Density Polyethylene for Blown Film
Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect..
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
SABIC FJ00952 High Density Polyethylene for Blown Film
Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, ..
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
SABIC BM1052 High Density Polyethylene for Blow Molding
Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im..
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene AM3245 PC High Density Polyethylene
CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS: PIPE EXTRUSIONSU..
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GA3245 High Density Polyethylene
CHARACTERISTICS: HIGH TOUGHNESS, GOOD EXTRUDABILITY, EXCELLENT IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR CARRIER BAGS, GROCERY BAGS, SHOPPING BAGS, INDUSTRIAL BAGS, LINER BAGS
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GA3750 High Density Polyethylene
CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GA3750 High Density Polyethylene
CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GG3245 High Density Polyethylene
CHARACTERISTICS: EXCELLENT ENVIRONMENTAL STRESS CRACKING RESISTANCE (ESCR) EXCELLENT IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH TOUGHNESSAPPLICATIONS: BLOW MOLDING/ SHEET/ THERMOFORMING EXTRUSION CO..