Physical Properties Metric English Comments
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Eraclene® BC 82 High Density Polyethylene - Blow Molding
Eraclene BC 82 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er..
Melt Flow 0.25 - 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 - 0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.25 - 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 - 0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6152C (526H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.25 - 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 - 0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.25 - 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 - 0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6949C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene AM3245 PC High Density Polyethylene
CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS: PIPE EXTRUSIONSU..
Melt Flow 0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GA3245 High Density Polyethylene
CHARACTERISTICS: HIGH TOUGHNESS, GOOD EXTRUDABILITY, EXCELLENT IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR CARRIER BAGS, GROCERY BAGS, SHOPPING BAGS, INDUSTRIAL BAGS, LINER BAGS
Melt Flow 0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GA3750 High Density Polyethylene
CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS
Melt Flow 0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GA3750 High Density Polyethylene
CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS
Melt Flow 0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene GG3245 High Density Polyethylene
CHARACTERISTICS: EXCELLENT ENVIRONMENTAL STRESS CRACKING RESISTANCE (ESCR) EXCELLENT IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH TOUGHNESSAPPLICATIONS: BLOW MOLDING/ SHEET/ THERMOFORMING EXTRUSION CO..
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HDPE HD 7800P High Density Polyethylene Copolymer Resin
Product Description: HD 7800P is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds..
Melt Flow 0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® HE3490-LS Black High Density Polyethylene for Pressure Pipes
Borstar HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding..