Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe PA 46 Nylon 46

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Unreinforced
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PA 46 Nylon 46.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality applications in plant engineering, electrical industry and in automotive industry.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 3.7 %
3.7 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 14 %
14 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 170 - 200 MPa

@Time 30.0 sec
24700 - 29000 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 65.0 MPa
9430 psi
cond.; DIN 53 455
80.0 MPa
11600 psi
dry; DIN 53 455
Elongation at Break 30 %
30 %
dry; DIN 53 455
280 %
280 %
cond.; DIN 53 455
Tensile Modulus 1.20 GPa
174 ksi
cond.; DIN 53 457
3.50 GPa
508 ksi
dry; DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.20 - 0.45
0.20 - 0.45
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 75.0 µm/m-°C
41.7 µin/in-°F
Specific Heat Capacity 2.10 J/g-°C
0.502 BTU/lb-°F
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Melting Point 295 °C
563 °F
DIN 53 736
Maximum Service Temperature, Air 140 °C
284 °F
Continuous use
280 °C
536 °F
Short Periods
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO-R 75 Method A
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
DIN 53 482, VDE 0303, Part 3
Dielectric Constant 9.4 - 11

@Frequency 1.00e+6 Hz
9.4 - 11

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength >= 20.0 kV/mm
>= 508 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.21 - 0.35

@Frequency 1.00e+6 Hz
0.21 - 0.35

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color reddish brown
Creep Resistance Grade CTI 400
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant in some conditions
Users viewing this material also viewed the following: