Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer A. Schulman, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Index of Compound 8.0 g/10 min

@Temperature 230 °C
8.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.4 MPa
4260 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Gardner Impact 15.02 J

@Thickness 3.20 mm,
Temperature -30.0 °C
11.08 ft-lb

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D3029