ExxonMobil LL 3201.69 Premium High Strength Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 3201.69 Premium High Strength Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, along with good drawdown capability, permit usage in many demanding packing applications.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: Yes Thermal Stabilizer: YesApplications: Freezer FilmGrocery SacksHeavy Duty BagsMerchandise Bags Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ExxonMobil Method
Thickness 38.1 microns
1.50 mil
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
Film Elongation at Break, MD 510 %
510 %
ASTM D882
Film Elongation at Break, TD 810 %
810 %
ASTM D882
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 30.7 g/micron
780 g/mil
ASTM D1922
Dart Drop 4.33 g/micron
110 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
Film Tensile Strength at Break, TD 48.3 MPa
7000 psi
ASTM D882
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
1% Secant Modulus, TD 283 MPa
41000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
Peak Melting Temperature; ExxonMobil Method
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Gloss 57 %
57 %
45°; ASTM D2457
Descriptive Properties Value Comments
Features Thermal Stabilizer
Users viewing this material also viewed the following: