Polymer Property : Puncture Energy = 2.94 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil
ExxonMobil LL 3003.32 Cast Film Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil
ExxonMobil LL 3003.39 Cast Film Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil
ExxonMobil LL 3201.69 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..