Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1327CA Blown Film Resin
(discontinued **) Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | ASTM D882 |
Westlake LF1050 Butene Linear Low Density Polyethylene Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade) Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | at 2% offset; ASTM D882 |
ExxonMobil LL 3201.36 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LL 3201.69 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | |
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | |
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | |
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl.. |
|||
Film Tensile Strength at Yield, MD | 11.7 MPa | 1700 psi | |
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl.. |