Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 48.3 - 96.5 MPa | 7000 - 14000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OEB (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Extra Barrier is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of .. |
|||
Film Tensile Strength at Break, TD | 48.3 - 96.5 MPa | 7000 - 14000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OEB (1.0 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Extra Barrier is a 1.00 (25micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relat.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil HDPE HTA 001HP2 High Density Polyethylene (HMW) Resin Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughn.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil LL 3201.36 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil LL 3201.69 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Film Tensile Strength at Break, TD | 48.3 MPa | 7000 psi | ASTM D882 |
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior p.. |