Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil Method |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil Method |
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil Method |
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil |
ExxonMobil LL 3003.32 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil |
ExxonMobil LL 3201.36 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil |
ExxonMobil LL 3201.69 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Puncture Energy | 2.94 J | 2.17 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |