Polymer Property : Elmendorf Tear Strength, MD = 5.51 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
ASTM D1922
ExxonMobil ESCOR™ AT 310 Blown Film Resin  (discontinued **)
ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo..
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
50 µm (2 mil) film; ASTM D1922
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des..
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
50 µm (2 mil) film; ASTM D1922
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol..
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
ASTM D1922
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
ASTM D1922
ExxonMobil LL 3201.69 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
ASTM D882
Dow INTEGRAL™ 917 Monolayer Bonding Film
INTEGRAL 917 Adhesive Film is a single layer adhesive film for use where a higher flow rate and lower melt point are required. It is useful for bonding heat sensitive materials, or for porous subst..
Elmendorf Tear Strength, MD 5.51 g/micron
140 g/mil
ASTM D882