Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc.. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil LDPE LD 158BW Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil LDPE LD 158JD Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil LL 3201.36 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil LL 3201.69 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
1% Secant Modulus, TD | 283 MPa | 41000 psi | ASTM D882 |
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A.. |