Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, TD = 13.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s..
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
ExxonMobil Exceed™ 1327HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength prope..
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula..
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
at 2% offset; ASTM D882
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
ExxonMobil LL 3201.69 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..