| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled , Nylon 66, Glass Fiber Filled, Flame Retardant , Nylon 66, Heat Stabilized |
| Manufacturer | Eurotec |
| Trade Name | Tecomid® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
| Moisture Absorption | 1.50 % @Temperature 23.0 °C |
1.50 % @Temperature 73.4 °F |
50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | Eurotec |
| Linear Mold Shrinkage, Transverse | 0.010 cm/cm | 0.010 in/in | Eurotec |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 140 MPa | 20300 psi | ISO 527 |
| Elongation at Break | 2.5 % | 2.5 % | ISO 527 |
| Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
| 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
| 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 262 °C | 504 °F | [10 K/min], ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 250 °C | 482 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 245 °C | 473 °F | ISO 75 |
| Flammability, UL94 | V-0 @Thickness 0.750 mm |
V-0 @Thickness 0.0295 in |
|
| V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
||
| Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI; IEC 60695 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Comparative Tracking Index | >= 350 V | >= 350 V | Solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
| Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | |
| Drying Temperature | 80.0 °C | 176 °F | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
| Moisture Content | <= 0.20 % | <= 0.20 % | ISO 960 |
| Hold Pressure | 50.0 - 100 MPa | 7250 - 14500 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Medium - Fast |