Zeon Chemicals Sivic® Z740 Polyblend Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Sivic®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Sivic® Z740 Polyblend Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sivic Z740 is a fully fluxed polyblend of 41% ACB NBR/PVC (70/30). IT is produced via a mechanical technology, which provides a lump-free homogenous polymer.High ACN content for improved fuel resistance in automotive applications.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Mooney Viscosity 45 - 57

@Temperature 100 °C
45 - 57

@Temperature 212 °F
(1+4)
Descriptive Properties Value Comments
Bound ACN (%, acrylonitrile) 41
NBR/PVC Ratio 70/30
Type PB