Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Thickness 4.00 mm,
Temperature 23.0 °C
3.81 ft-lb/in²

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180/1A
Polimeri Europa Edistir RT 441M Polystyrene
High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers. Especially rec..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Thickness 4.00 mm,
Temperature -40.0 °C
3.81 ft-lb/in²

@Thickness 0.157 in,
Temperature -40.0 °F
ISO 180/1A
Polimeri Europa Sinkral® E 332 ABS Resin
Sinkral E 332 is a medium heat injection molding grade offering good flow and good impact resistance together with an excellent thermal stability during processing. Designation: Thermoplastic ISO 2..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East)
CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT
Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy XP4034 ASA (Europe-Africa-Middle East)
GELOY XP4034 is a high heat modified ASA+PC alloy. It is a weatherable, injection mouldable product which is available in a wide range of colours. The product is recommended for automotive unpainted..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® 2014R PC (Europe-Africa-Middle East)
LEXAN 2014R is a medium viscosity flame retardant grade, This material contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region...
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -20.0 - -20.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 8.00 kJ/m² Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Thickness 4.00 - 4.00 mm
3.81 - 3.81 ft-lb/in²

@Thickness 0.157 - 0.157 in
Average value: 8.00 kJ/m² Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® ML3019 PC (Europe-Africa-Middle East)
LEXAN ML3019 is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications like industrial enclosures and fuse boxes requiring a low knock-out strength for..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East)
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/A
Styrolution Novodur® H702 ABS
Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East)
30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1A
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded
AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Staramide BG6ST01 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG6ST01 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
80x10x4; ISO 180/1A
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecodur® PB70 GR15 NL TD 28 PBT 15% glass fiber reinforced, UL94 V0, impact modified, high CTI
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NA40 KK30 NL PA 6.6 30% glass fiber/mineral reinforced, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1A
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded
BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1A
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecopet® PT74 GR30 BK002 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black
Information provided by Eurotec®
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate
SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.Information provided by SAX Polymers
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -40.0 °C
3.81 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
DuPont Performance Polymers Crastin® HR5330HF BK503 PBT  (Unverified Data**)
Crastin® HR5330HF is a 30% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled
SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers