Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Eurostar Engineering Plastics
Trade Name Starflam
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Water Absorption at Saturation 4.5 %

@Temperature 23.0 °C
4.5 %

@Temperature 73.4 °F
ISO 62-1
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
on Tensile Bar; E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
5 mm/min; ISO 527
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
Tensile Modulus 9.10 GPa
1320 ksi
1 mm/min; ISO 527
Flexural Strength 215 MPa
31200 psi
2 mm/min; ISO 178
Flexural Modulus 8.90 GPa
1290 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
80x10x4; ISO 180/1A
7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
16.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 256 °C
493 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Ae
Vicat Softening Point 255 °C
491 °F
B/120; ISO 306
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Comparative Tracking Index 375 V
375 V
IEC 60112
Processing Properties Metric English Comments
Zone 1 260 - 270 °C
500 - 518 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 270 - 285 °C
518 - 545 °F
Melt Temperature 270 - 285 °C
518 - 545 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Moisture Content 0.20 %
0.20 %