Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ASTM D1525 |
Nilit Polynil® P36 Very High Flow Nylon 66 Description: Very high flowApplication: CompoundingInformation provided by NILIT. |
|||
Vicat Softening Point | 255 °C | 491 °F | 9.8 N; ASTM D1525 |
Nilit Polynil® P50FI Internally Lubricated Nylon 66 Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Oil stabilized. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Vicat Softening Point | 255 °C | 491 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1/CF/30/TF/15 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Vicat Softening Point | 255 °C | 491 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Vicat Softening Point | 255 °C | 491 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers |
|||
Vicat Softening Point | 255 °C | 491 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Vicat Softening Point | 255 °C | 491 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP RC003SXS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC003SXS is a compound based on PA 66 resin containing Carbon fiber. Added features include: Electrically Conductive, Heat Stabilized |
|||
Vicat Softening Point | 255 °C | 491 °F | ISO 306 |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide AK6 PA66, 30% Mineral Reinforced, Injection Molding Staramide AK6 is a 30% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
Eurostar Staramide AS10 PA66, 50% Glass Bead Reinforced, Injection Molding Staramide AS10 is a 50% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR30 NL RM PA 6.6 30% glass fiber reinforced, low friction and wear Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR30 NL RM PA6.6, 30% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR30 NL RT PA 6.6 30% glass fiber reinforced, very low friction and wear Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR40 NL PA 6.6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 255 °C | 491 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 GR20 NL PA 6.6 20% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Vicat Softening Point | 255 °C @Load 5.00 kg |
491 °F @Load 11.0 lb |
|
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |
|||
Vicat Softening Point | 255 °C | 491 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |