Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527 |
Grupo Repol Dinalon® B1X25 G30W PA6 30% Glass Fiber, Reduced Water Abs. Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | |
LATI Latilub 66-10T K/10 PA66, 10% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefit.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Asia Pacific) LNP* Thermocomp* DF006 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF0069P PC LNP THERMOCOMP* DF0069P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF005 PA 66 LNP* THERMOCOMP* RF005 is a compound based on Nylon 66 resin containing 25% Glass Fiber. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RF005 PA 66 (Asia Pacific) LNP* Thermocomp* RF005 is a compound based on Nylon 66 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East) VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Plenco 4304 Phenolic, Nodular, Transfer Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | Longitudinal |
Goodfellow Polyethylene Fiber/Polyethylene composite Information provided by Goodfellow. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Plenco 4311 Phenolic, Granular, Injection Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | |
Covestro Baygal® 90 IK 20 Polyurethane Uses: Suitable for the production of parts: for example: insulators, bushing insulators, components of switchgear cabinets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1010G30 NA PA6-GF30 30% Glass Reinforced, Injection Molding, Easy Molding Grade, High Flow |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ASTM D638 |
Plenco 4311 Phenolic, Granular, Transfer Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | |
LATI Latimass 62-01 D025 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Tensile Modulus | 9.10 GPa | 1320 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **) Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, .. |