Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Elastomer Engineering
Trade Name Elastamide
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
29% crystallinity. Information supplied by Elastomer Engineering.
Physical Properties Metric English Comments
Water Absorption 2.5 %
2.5 %
24 hrs; DIN 53714
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 320 %
320 %
ASTM D638
Tensile Modulus 0.900 GPa
131 ksi
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 6.03 J/cm
11.3 ft-lb/in
Method B; Ductile Failure
1.01 J/cm

@Temperature -40.0 °C
1.89 ft-lb/in

@Temperature -40.0 °F
Method B; Brittle Failure
Charpy Impact, Notched 1.65 J/cm²
7.85 ft-lb/in²
Ductile Failure; ASTM D256B
0.600 J/cm²

@Temperature -40.0 °C
2.86 ft-lb/in²

@Temperature -40.0 °F
Method B; Brittle Failure
Electrical Properties Metric English Comments
Dielectric Constant 4.2

@Frequency 100000 Hz
4.2

@Frequency 100000 Hz
7.8

@Frequency 1000 Hz
7.8

@Frequency 1000 Hz
14.9

@Frequency 50 Hz
14.9

@Frequency 50 Hz
Dielectric Strength 13.0 kV/mm
330 kV/in
Dissipation Factor 0.10

@Frequency 100000 Hz
0.10

@Frequency 100000 Hz
ASTM D150
0.30

@Frequency 1000 Hz
0.30

@Frequency 1000 Hz
ASTM D150
Comparative Tracking Index 500 V
500 V
ASTM D257