Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 44.0 MPa @Temperature 120 °C |
6380 psi @Temperature 248 °F |
ISO 527 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Hannam Chemical Hanalac 710 ABS |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | |
Ineos Styrenics Polystyrene 148G (NAFTA) High heat, easy flow general purpose polystyrene with excellent clarity. Designed for applications requiring a combination of fast processing with good strength and heat resistance.Information prov.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
KYDEX® 6185 Thermoplastic Sheet High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE) Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® F 7 Polytetrafluoroethylene (PTFE) Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 5350 Phenolic, Granular, Injection Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6 29% crystallinity. Information supplied by Elastomer Engineering. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TG 615 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TG 617 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo A2064D Thermoplastic Polyurethane Elastomer, Injection Grade Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 4002 Phenolic, Granular, Injection Molded PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo A3064D Thermoplastic Polyurethane Elastomer, Injection Grade Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo E1095A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527 |
DSM Fibre Intermediates Nyrim® 1500 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO R527 |
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 44.0 MPa @Temperature 1093 °C |
6380 psi @Temperature 1999 °F |
ASTM E8 |
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS 220 High impact for extrusion. Applications: Extrusion sheet applications including refrigerator door liners and inner box liners, picnic coolers, snow boats, luggage cases, etc.Data provided by the m.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527B |
Ineos Nova 212 Crystal Polystyrene Low Flow Grade
(discontinued **) Excellent balance of properties; Extrusion and Injection MoldingApplications: Foam insulation, XPS food packaging, Sheet and profile extrusion, CD and DVD jewel boxesProperties were determined on i.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS Resin F-221 High gloss, high impact, extrusion grade.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® P268WO PPO An extrusion grade for general purpose application requiring flame retardancy and good impact resistance.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527B |
Ineos Nova 204L Crystal Polystyrene General Purpose Grade
(discontinued **) Fast cycling, Good heat resistance, Good balance of properties and flow characteristics, Extrusion and Injection Molding Applications: General purpose injection molded itemsProperties were determin.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527B |
Ineos Nova 207 Crystal Polystyrene High Heat, High Flow Grade
(discontinued **) Fast cycling, Excellent flow characteristics, Extrusion and Injection Molding Applications: XPS sheet, Foam insulation, CD and DVD jewel boxesProperties were determined on injection molded specimen.. |
|||
Tensile Strength, Ultimate | 44.0 - 55.0 MPa | 6380 - 7980 psi | Average value: 50.6 MPa Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |