Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.03 J/cm | 11.3 ft-lb/in | ASTM D256 |
Flint Hills P6G2N-095 Impact Copolymer Polypropylene Features: Excellent stiffness and impact resistance, nucleated, suitable for retort and hot fill applications. Product does not contain animal derived components.Applications: Blow molding, sheet/.. |
|||
Izod Impact, Notched | 6.03 J/cm | 11.3 ft-lb/in | ASTM D-256 |
Glastic 1130 Angles, Channels, and Structural Shapes Information provided by Glastic Corporation |
|||
Izod Impact, Notched | 6.03 J/cm | 11.3 ft-lb/in | Method B; Ductile Failure |
Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6 29% crystallinity. Information supplied by Elastomer Engineering. |
|||
Izod Impact, Notched | 6.03 J/cm | 11.3 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 522 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Izod Impact, Notched | 6.03 J/cm | 11.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 LNP* STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Notched | 6.03 J/cm | 11.3 ft-lb/in | ASTM D-256 |
Glastic GLASGUARD 1130 Corrosion-Resistant Panels GlasGuard Grade 1130 is a fiberglass-reinforced thermoset polymer composite system which is available as sheet stock or in a variety of pultruded shapes. Grade 1130 possesses flame resistance, corr.. |
|||
Izod Impact, Notched | 6.03 J/cm | 11.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 (Asia Pacific) LNP STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |