Polymer Property : Charpy Impact, Notched = 1.65 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.65 J/cm²
7.85 ft-lb/in²
Ductile Failure; ASTM D256B
Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6
29% crystallinity. Information supplied by Elastomer Engineering.
Charpy Impact, Notched 1.65 J/cm²

@Temperature 23.0 °C
7.85 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..