Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.0 - 19.0 kV/mm | 330 - 483 kV/in | ASTM D149 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149 |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Dielectric Strength | 13.0 - 120 kV/mm | 330 - 3050 kV/in | Average value: 25.5 kV/mm Grade Count:20 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Dielectric Strength | 13.0 - 70.0 kV/mm | 330 - 1780 kV/in | Average value: 26.1 kV/mm Grade Count:52 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149 |
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 45U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Dielectric Strength | 13.0 kV/mm @Thickness 3.00 mm |
330 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Beetle® MD21 Nylon 6, Extrusion Grade Notes: MD21 is a medium viscosity grade of nylon 6, designed for wire coating extrusion. MD21 is heavily pigment and is designed to provide good opacity even with thin coatings. It also features a.. |
|||
Dielectric Strength | 13.0 kV/mm @Thickness 3.00 mm |
330 kV/in @Thickness 0.118 in |
IEC 243 |
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic RX 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | Wet, Step by Step |
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | |
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6 26% crystallinity. Information supplied by Elastomer Engineering. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149-95a |
Thermoseal KLINGERSIL® C-4324 Compressed Inorganic Fiber Gasketing Recycled Fiberglass & Aramid BlendNitrile BinderLow Pressure Steam, Water & GasesGood for Oils and FuelsInformation provided by Thermoseal Inc. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | Wet, Step by Step |
Cosmic Plastics E4905 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Dielectric Strength | 13.0 kV/mm | 329 kV/in | |
Dow Corning SE 4486 SILICONE RTV One-part, white, moisture cure RTV, highly flowable, fast tack-free, high thermal conductivity, controlled volatility.Information provided by Dow Corning |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149 |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 55 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | DIN 53481 |
DSM Fibre Intermediates Nyrim® 1500 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | DIN 53481 |
Brueggemann Chemical Nyrim® 1000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | Short Time |
Bulk Molding Compounds BMC 3001H Mineral Filled Alkyd BMC 3001H molding compound is a mineral filled, glass-fiber reinforced alkyd compound suitable for compression and transfer molding. Because of its soft flow, it is also used extensively in cold spu.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | Short Time |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | Short Time |
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | Short Time; Dry; ASTM D149 |
Resinoid 1360 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149 |
Plaslok 5440 Black General Purpose Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5440 is the replacement material for .. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | Wet, Step by Step |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149 |
Plaslok 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 501 is a two-stage, mineral and flock.. |
|||
Dielectric Strength | 13.0 kV/mm | 330 kV/in | ASTM D149-97 |
Saint-Gobain Tygothane® C-210-A Precision Polyurethane Tubing Formulation Description: Tygothane® C-210-A: Our rigidly controlled manufacturing process makes Tygothane® Precision Polyurethane Tubing the flexible polyurethane tubing that has consistently tight toleranc.. |