Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638-61T |
Rotuba 860H Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 44.0 MPa @Temperature 120 °C |
6380 psi @Temperature 248 °F |
ISO 527 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Global GA-2850 High Density Polyethylene, Blow Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containersMeets FDA requirements as listed in food add.. |
|||
Tensile Strength, Ultimate | 44.0 - 130 MPa | 6380 - 18900 psi | Average value: 66.4 MPa Grade Count:15 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Hannam Chemical Hanalac 710 ABS |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
KYDEX® 6185 Thermoplastic Sheet High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE) Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 4300 Phenolic, Granular, Compression Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 5350 Phenolic, Granular, Injection Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6 29% crystallinity. Information supplied by Elastomer Engineering. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TG 615 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Tipco Tipcolite® TX 312 Phenolic Compound, Wood Flour & Minerals having Soft Flow & Lower Density Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | |
Williams Advanced Alloys WS179 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Plenco 4002 Phenolic, Granular, Injection Molded PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D638 |
Toyobo E1095A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 37 |
Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO 527 |
DSM Fibre Intermediates Nyrim® 1500 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ISO R527 |
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS 220 High impact for extrusion. Applications: Extrusion sheet applications including refrigerator door liners and inner box liners, picnic coolers, snow boats, luggage cases, etc.Data provided by the m.. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | 20 in/min, at max load; ASTM D412 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® ABS Resin F-221 High gloss, high impact, extrusion grade.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ATSM D638 |
Ashley Polymers Ashlene® P268WO PPO An extrusion grade for general purpose application requiring flame retardancy and good impact resistance.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 44.0 MPa | 6380 psi | ASTM D651 |
Resinoid 2018 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |