Ecomass® 706BI76 Filled ABS, Injection Molding Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Plating Grade
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 706BI76 Filled ABS, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moderate Specific Gravity, Filled ABS, Plating Grade, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to traditional materialsInformation provided by Technical Polymers.
Physical Properties Metric English Comments
Specific Gravity 2.50 g/cc
2.50 g/cc
ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength 20.0 MPa
2900 psi
ISO 527
Elongation at Break 3.0 - 5.0 %
3.0 - 5.0 %
ISO 527
Flexural Modulus 5.47 GPa
793 ksi
ISO 178
Izod Impact, Notched 0.640 J/cm

@Thickness 3.20 mm
1.20 ft-lb/in

@Thickness 0.126 in
ISO 180-A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
ISO 75
Vicat Softening Point 97.0 °C
207 °F
ISO 306
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 220 - 265 °C
428 - 509 °F
Mold Temperature 50.0 - 80.0 °C
122 - 176 °F
Drying Temperature 90.0 °C
194 °F
Dry Time 2 - 4 hour
2 - 4 hour