Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.47 GPa | 793 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Flexural Modulus | 5.47 GPa | 793 ksi | ASTM D790 |
Kostat 7440 Conductive ABS Compound KOSTAT 7440 is a conductive thermoplastic compound based on Acrylonitrile Butadiene Styrene and a special carbon black. KOSTAT 7440 is not dependant on atmospheric conditions and is used for ESD in.. |
|||
Flexural Modulus | 5.47 GPa | 793 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66 LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Flexural Modulus | 5.47 GPa | 793 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Modulus | 5.47 GPa | 793 ksi | ISO 178 |
Ecomass® 706BI76 Filled ABS, Injection Molding Grade Moderate Specific Gravity, Filled ABS, Plating Grade, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to traditional materialsInformation provided by Technical Polyme.. |