Material Notes:
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental
Physical Properties Metric English Comments
Density 14.1 g/cc
0.509 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 210
210
HV5/30; after porcelain firing
240
240
HV5/30; hardened
Tensile Strength, Yield 489.9 MPa

@Strain 0.200 %
71050 psi

@Strain 0.200 %
after porcelain firing
529.9 MPa

@Strain 0.200 %
76850 psi

@Strain 0.200 %
hardened
Elongation at Break 12 %
12 %
hardened
14 %
14 %
after porcelain firing
Modulus of Elasticity 114 GPa
16500 ksi
Thermal Properties Metric English Comments
CTE, linear 14.7 µm/m-°C

@Temperature 25.0 - 500 °C
8.17 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Gold, Au 51.5 %
51.5 %
Indium, In 0.90 %
0.90 %
Palladium, Pd 26.6 %
26.6 %
Ruthenium, Ru 0.10 %
0.10 %
Silver, Ag 18.2 %
18.2 %
Tin, Sn 2.7 %
2.7 %
Processing Properties Metric English Comments
Processing Temperature 849 °C
1560 °F
Preheating Temp.
Melt Temperature 1200 - 1280 °C
2190 - 2330 °F
Casting Temperature 1400 °C
2550 °F
Descriptive Properties Value Comments
Color white