Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | 120°C/h; ASTM D 648 |
Polimeri Europa Edistir N 2560 Polystyrene High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet
extrusion in ble.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 3.20 mm |
183 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYasa 2410F High Flow ASA Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C6200 is a non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. C6200 has improved processing window and edge crac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 3.20 mm |
183 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Geloy FXTW26SK ASA Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP FARADEX KS002E Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KS002E is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Electrically Conductive, Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | ASTM D648 |
Albis Plastics ASA 02A 811 Unreinforced
(discontinued **) Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 6.40 mm |
183 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed (0.5"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ ABS-0500RX Biocompatible ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed (0.5"); ASTM D648 |
LTL Color Compounds ColorRxâ„¢ ABS-0502AF Food Grade ABS A high gloss, injection molding grade of ABS with FDA food contact approval, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 6.35 mm |
183 °F @Thickness 0.250 in |
ASTM D648 |
IRPC Polimaxx Porene SP200 Acrylonitrile Butadiene Styrene Applications:injection moldingHelmetsautomotiveelectroplatingpainting articles |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 6.40 mm |
183 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 6.40 mm |
183 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® VS-0826 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 6.40 mm |
183 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | Unannealed; ISO 75-2/A |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 3.20 mm |
183 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Stat-kon AD000Z ABS LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C @Thickness 6.40 mm |
183 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | 80*10*4 s=60mm; ISO 75-1 a |
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | |
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe) Heat distortion resistant, good flowing grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs H00 ABS, Heat Resistant Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | |
Polimeri Europa SINKRAL PD G120 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-09-30 General purpose injection moulding grade. Characteristics: outstanding rigidity very high surface.. |