Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade

Category Polymer , Thermoplastic , Polyether Block Amide (PEBA)
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding applicationsInformation provided by Technical Polymers.
Physical Properties Metric English Comments
Specific Gravity 11.0 g/cc
11.0 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 19.0 MPa
2750 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D638
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Flexural Modulus 0.758 GPa
110 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 51.7 °C
125 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 232 - 260 °C
450 - 500 °F
Mold Temperature 65.6 - 82.2 °C
150 - 180 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 4 hour
4 hour
Copyright © lookpolymers.com All Rights Reserved