Polymer Property : Tensile Strength = 2750 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 19.0 MPa
2750 psi
ASTM D638
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio..
Tensile Strength 19.0 MPa
2750 psi
AlphaGary Garaflex™ G 7782-A4 Thermoplastic Elastomer
Garaflex™ G is a thermoplastic elastomer intended for wire and cable applications105°C rated TPE for flexible cord (SEO & SJEO).
Tensile Strength 19.0 MPa
2750 psi
2 in/min; ASTM D638
Braskem TI6120Q4 High Impact Copolymer Polypropylene
Description: Extra High Izod Impact, Superior Low Temperature Drop Impact, Good Paint AdhesionApplications: Suggested Uses Include Compounding, Automotive, Injection MoldingThis resin meets the requ..