Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Spectar® Clear Copolyester for Thermoforming

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Spectar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Spectar® Clear Copolyester for Thermoforming.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Decorative Light-Transmitting PanelsHeavy gauge sheet displaysKey Attributes:Easy to print and decorateExcellent clarityExcellent thermoforming characteristicsGood chemical resistanceOdorlessOutstanding impact resistanceOutstanding toughness allows downgaugingResists chipping and crackingVersatile - easy to fabricateProduct Description: Eastman Spectar Clear is a copolyester, developed by Eastman to achieve measurably improved sheet clarity and edge color while maintaining high performance characteristics. It offers the thermoformability and ease of fabrication of Eastman Spectar copolyester along with significantly improved clarity. Eastman Spectar Clear also offers approximately double the notch impact strength, 50% higher instrumented impact strength and better chemical resistance when compared to traditional Spectar Copolyester. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.Information provided by Eastman.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D1505
Water Absorption 0.19 %
0.19 %
Immersion; ASTM D570
Viscosity Measurement 0.73
0.73
Inherent; EMN-A-AC-G-V-1
Thickness 3000 microns
118 mil
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength at Break 53.0 MPa
7690 psi
ASTM D638
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 340 %
340 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM D638
Flexural Strength 71.0 MPa

@Strain 5.00 %
10300 psi

@Strain 5.00 %
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.830 J/cm

@Temperature -30.0 °C
1.55 ft-lb/in

@Temperature -22.0 °F
ASTM D256
1.13 J/cm

@Temperature 0.000 °C
2.12 ft-lb/in

@Temperature 32.0 °F
ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ASTM D4812
Puncture Energy 41.0 J

@Temperature 23.0 °C
30.2 ft-lb

@Temperature 73.4 °F
At Max load; ASTM D3763
42.0 J

@Temperature 0.000 °C
31.0 ft-lb

@Temperature 32.0 °F
At Max load; ASTM D3763
52.0 J

@Temperature -30.0 °C
38.4 ft-lb

@Temperature -22.0 °F
At Max load; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 76.2 µm/m-°C
42.3 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
ASTM D648
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Flammability, UL94 V-2
V-2
Optical Properties Metric English Comments
Haze 0.50 %
0.50 %
ASTM D1003
Gloss 150 %
150 %
at 60°; ASTM D2457
Yellow Index 0.81 %
0.81 %
ASTM E313
Transmission, Visible 91 %
91 %
Total; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+17 ohm
1.00e+17 ohm
ASTM D257
Arc Resistance 130 sec
130 sec
ASTM D495
Descriptive Properties Value Comments
Static Decay Failed to discharge
ASTM D4470
Copyright © lookpolymers.com All Rights Reserved