Material Notes:
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good chemical resistanceGood flow and processing propertiesAPPLICATIONS: AutomotiveElectrical/ElectronicFurnitureConstructionHome appliances
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Filler Content 15 %
15 %
ISO 3451
Moisture Absorption at Equilibrium 1.7 %
1.7 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 6.0 %
6.0 %
23°C; ISO 62
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75-1/2
Vicat Softening Point 255 °C
491 °F
50N; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
plaque; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 250 V
250 V
IEC 60112