Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
PolyOne Lubri-Tech™ ATH-000/5T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
Eastman Spectar® Clear Copolyester for Thermoforming Applications:Decorative Light-Transmitting PanelsHeavy gauge sheet displaysKey Attributes:Easy to print and decorateExcellent clarityExcellent thermoforming characteristicsGood chemical resistanceOd.. |
|||
Surface Resistivity per Square | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
Eastman TiGlaze SV Copolyester TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh.. |
|||
Surface Resistivity per Square | 1.00e+17 ohm | 1.00e+17 ohm | in air; ASTM D257 |
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T.. |
|||
Surface Resistivity per Square | 1.00e+17 ohm | 1.00e+17 ohm | in air; ASTM D257 |
DuPont™ Nomex® Type 994, 250 mil Nominal Thickness Rigid Aromatic Nylon Board Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T.. |
|||
Surface Resistivity per Square | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
Arkema Group Pebax® MH 2030 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MH 2030 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 2030 is an inherently dissipative polymer and can be dry blended or compounded w.. |