DuPont™ Surlyn® 8660 Ionomer Resin, Sodium

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer DuPont
Trade Name Surlyn®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Surlyn® 8660 Ionomer Resin, Sodium.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn® 8660 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neutralization levels for this grade are optimized for ease of compounding with high loadings of various color pigments. The resin is easily injection molded, and also is used in foamed applications. It complies with the provisions of U.S. Food and Drug Administration (FDA) Title 21 Code of Regulations 177:1330 - ionomer resins.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength, Ultimate 23.4 MPa
3390 psi
ASTM D638
Tensile Strength, Yield 13.1 MPa
1900 psi
50 mm/min cross speed; ASTM D638
Elongation at Break 470 %
470 %
ASTM D638
Flexural Modulus 0.230 GPa
33.4 ksi
ASTM D790
Izod Impact, Notched 8.55 J/cm
16.0 ft-lb/in
ASTM D256
Tensile Impact Strength 730 kJ/m²
347 ft-lb/in²
ASTM D1822S
Abrasion 170
170
NBS Index; ASTM D1630
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C

@Temperature -20.0 - 32.0 °C
83.3 µin/in-°F

@Temperature -4.00 - 89.6 °F
ASTM D696
Thermal Conductivity 0.246 W/m-K
1.71 BTU-in/hr-ft²-°F
Melting Point 95.0 °C
203 °F
DTA
Deflection Temperature at 0.46 MPa (66 psi) 42.0 °C
108 °F
ASTM D648
Vicat Softening Point 71.0 °C
160 °F
Rate B, ASTM D1525-70
Brittleness Temperature -75.0 °C
-103 °F
ASTM D746
Flame Spread 25.4 mm/min
1.00 in/min
ASTM D635
Optical Properties Metric English Comments
Haze 11 %

@Thickness 6.40 mm
11 %

@Thickness 0.252 in
ASTM D1003A