Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.247 W/m-K | 1.71 BTU-in/hr-ft²-°F | ASTM D435 |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Thermal Conductivity | 0.246 W/m-K | 1.71 BTU-in/hr-ft²-°F | |
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Thermal Conductivity | 0.246 W/m-K | 1.71 BTU-in/hr-ft²-°F | |
DuPont™ Surlyn® 8660 Ionomer Resin, Sodium Surlyn® 8660 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Thermal Conductivity | 0.246 W/m-K | 1.71 BTU-in/hr-ft²-°F | |
DuPont™ Surlyn® 8940 Ionomer Resin, Sodium Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Thermal Conductivity | 0.246 W/m-K | 1.71 BTU-in/hr-ft²-°F | |
DuPont™ Surlyn® 9650 Ionomer Resin, Zinc Surlyn® 9650 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |