Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Henkel Hysol EA 9258.1 Primer

Category Polymer , Thermoset
Manufacturer Henkel
Trade Name Hysol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9258.1 Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Waterborne, corrosion-inhibiting primer, designed to provide enhanced toughness and high temperature performance where continuous exposures up to 350°F / 177°C are required. Meets SCAQMD Rule 1124.Applications: Sprayable Low Viscosity Wet Lay-up Metal and Honeycomb Bonding
Physical Properties Metric English Comments
Storage Temperature 5.00 °C
41.0 °F
Mechanical Properties Metric English Comments
Tensile Strength 7.00 MPa
1020 psi
Flatwise
Adhesive Bond Strength 19.0 MPa

@Temperature 177 °C
2760 psi

@Temperature 351 °F
Lap Shear
27.0 MPa

@Temperature -55.0 °C
3920 psi

@Temperature -67.0 °F
Lap Shear
33.0 MPa

@Temperature 22.0 °C
4790 psi

@Temperature 71.6 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 177 °C
1.00 hour

@Temperature 351 °F
Descriptive Properties Value Comments
Honeycomb Climbing Drum Peel, mN/m 60
at 25°C
Out-Time (days) 30
at 25°C
Primer Coverage, sq.m/L 416
at 8µm dry film thickness
Copyright © lookpolymers.com All Rights Reserved