Mechanical Properties Metric English Comments
Flexural Modulus 0.230 GPa
33.4 ksi
ASTM D790
ExxonMobil Escorene® LD-421 LDPE Power Cable Insulation  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer designed as an electrical grade base resin.Applications: A base resin for fully formulated crosslinkable me..
Flexural Modulus 0.230 - 3.50 GPa
33.4 - 508 ksi
Average value: 2.23 GPa Grade Count:44
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Flexural Modulus 0.230 GPa
33.4 ksi
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Modulus 0.230 GPa
33.4 ksi
1% secant at 0.05 in/min; ASTM D790A
LyondellBasell Adflexâ„¢ KS-021P TPO Resin
Primary Processing Method: Blown Film/Impact ModificationKey Features: excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, FDA acceptable, n..
Flexural Modulus 0.230 GPa
33.4 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer
LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant.
Flexural Modulus 0.230 GPa
33.4 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East)
LNP* LUBRICOMP* YL003 is a compound based on Polyester Elastomer containing PTFE. Added features include; Internally Lubricated.
Flexural Modulus 0.230 GPa
33.4 ksi
ASTM D790
Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.
Flexural Modulus 0.230 GPa
33.4 ksi
ISO 178
Chengdu Polyster FH605 Thermoplastic Polyether-ester Elastomer (TPEE)
Blend of H605 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by ..
Flexural Modulus 0.230 GPa
33.4 ksi
ASTM D790
DuPont™ Surlyn® 8660 Ionomer Resin, Sodium
Surlyn® 8660 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Flexural Modulus 0.230 GPa
33.4 ksi
Conditioned; ISO 178
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66  (discontinued **)
PA 6/66