Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Impact Modified
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high melt viscosity. It was previously coded Zytel FE240012Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
DAM; ISO 1183
Viscosity 82000 cP

@Shear Rate 5000 1/s,
Temperature 270 °C
82000 cP

@Shear Rate 5000 1/s,
Temperature 518 °F
ISO 11403-1 -2
98500 cP

@Shear Rate 5000 1/s,
Temperature 250 °C
98500 cP

@Shear Rate 5000 1/s,
Temperature 482 °F
ISO 11403-1 -2
110700 cP

@Shear Rate 5000 1/s,
Temperature 240 °C
110700 cP

@Shear Rate 5000 1/s,
Temperature 464 °F
ISO 11403-1 -2
292700 cP

@Shear Rate 500 1/s,
Temperature 270 °C
292700 cP

@Shear Rate 500 1/s,
Temperature 518 °F
ISO 11403-1 -2
369700 cP

@Shear Rate 500 1/s,
Temperature 250 °C
369700 cP

@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
403800 cP

@Shear Rate 500 1/s,
Temperature 240 °C
403800 cP

@Shear Rate 500 1/s,
Temperature 464 °F
ISO 11403-1 -2
Linear Mold Shrinkage, Flow 0.026 cm/cm
0.026 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
50%RH; ISO 527-1/-2
32.0 MPa
4640 psi
DAM; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
DAM; Nominal; ISO 527-1/-2
>= 50 %
>= 50 %
50%RH; Nominal; ISO 527-1/-2
Elongation at Yield 12 %
12 %
DAM; ISO 527-1/-2
30 %
30 %
50%RH; ISO 527-1/-2
Tensile Modulus 0.750 GPa
109 ksi
50%RH; ISO 527-1/-2
1.10 GPa
160 ksi
DAM; ISO 527-1/-2
Shear Strength 0.04481 MPa

@Shear Rate 50.0 1/s,
Temperature 270 °C
6.499 psi

@Shear Rate 50.0 1/s,
Temperature 518 °F
ISO 11403-1 -2
0.05407 MPa

@Shear Rate 50.0 1/s,
Temperature 250 °C
7.842 psi

@Shear Rate 50.0 1/s,
Temperature 482 °F
ISO 11403-1 -2
0.05737 MPa

@Shear Rate 50.0 1/s,
Temperature 240 °C
8.321 psi

@Shear Rate 50.0 1/s,
Temperature 464 °F
ISO 11403-1 -2
0.14635 MPa

@Shear Rate 500 1/s,
Temperature 270 °C
21.226 psi

@Shear Rate 500 1/s,
Temperature 518 °F
ISO 11403-1 -2
0.18485 MPa

@Shear Rate 500 1/s,
Temperature 250 °C
26.810 psi

@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
0.2019 MPa

@Shear Rate 500 1/s,
Temperature 240 °C
29.28 psi

@Shear Rate 500 1/s,
Temperature 464 °F
ISO 11403-1 -2
0.410 MPa

@Shear Rate 5000 1/s,
Temperature 270 °C
59.5 psi

@Shear Rate 5000 1/s,
Temperature 518 °F
ISO 11403-1 -2
0.4925 MPa

@Shear Rate 5000 1/s,
Temperature 250 °C
71.43 psi

@Shear Rate 5000 1/s,
Temperature 482 °F
ISO 11403-1 -2
0.5535 MPa

@Shear Rate 5000 1/s,
Temperature 240 °C
80.28 psi

@Shear Rate 5000 1/s,
Temperature 464 °F
ISO 11403-1 -2
Charpy Impact, Notched 3.50 J/cm²
16.7 ft-lb/in²
DAM; ISO 179/1eA
8.00 J/cm²
38.1 ft-lb/in²
50%RH; ISO 179/1eA
1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C
117 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >PA612-HI<
ISO 11469
Processing Blow Moulding
Other Extrusion
Profile Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA612-HI
PA612-HI
ISO 1043
Special Characteristics Heat stabilised or stable to heat