Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 82000 cP @Shear Rate 5000 1/s, Temperature 280 °C |
82000 cP @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Viscosity | 82000 cP @Shear Rate 5000 1/s, Temperature 270 °C |
82000 cP @Shear Rate 5000 1/s, Temperature 518 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high .. |
|||
Viscosity | 82000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
82000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ 2535 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2535 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and stress crack resistance with good flexibility. It has good proces.. |
|||
Viscosity | 82000 cP @Shear Rate 1000 1/s, Temperature 190 °C |
82000 cP @Shear Rate 1000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ IP-10262 High Density Polyethylene DOWLEX® IP-10262 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution for use in reusable case applications including, poultry, fast food, a.. |