Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.750 GPa | 109 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® EQ 18 N Polyethylene Impact modified PE for extrusion. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data) TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | |
Radici Radilon® CS 38FL (cond.) Nylon 6/66 Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | DIN 53457 |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP 1802 H3.0 000000 Nylon 6 PA 6 injection and extrusion molding grade, non-reinforced, impact-modified, UL 94V-2 off 0,75 mm, GWIT: 775°C off 0,75 mm, halogen-free |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6 PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | DIN 53457 |
Isoflon PEHD 300 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | |
LATI Latiblend 5262 PP Homopolymer/PA6 Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 HL X black 9992 PA610 Product Description: Grilamid 2S 25 W 20 HL X black 9992 is a semi-flexible high viscosity heat stabilized, impact modified and plasticized Polyamide 610, especially suitable for extrusion applicati.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610 Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 X black 9992 PA610-I Product Description: GRILAMID 2S 25 W 20 X black 9992 is a semi-flexible high viscosity heat and impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is .. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® F 34 NL PA6 Grilon F 34 NL nat. 6019 is a medium viscosity PA 6 containing nucleation and lubrication suitable for the production of coex blown films and mono or coex cast films. Grilon F 34 NL nat. 6019 has be.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6 Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSS PA666 Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSZ 1 PA666 Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow beha.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high .. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® F 40 NL PA6 Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® F 47 NL nat 6028 PA6 Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | ISO 527 |
Eurotec® Tecolen® CP30 NL MY PPCP, impact modified, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 0.750 GPa @Temperature 80.0 °C |
109 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Tensile Modulus | 0.750 GPa @Temperature 80.0 °C |
109 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8202C PA6 (Dry) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |
|||
Tensile Modulus | 0.750 GPa | 109 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |