Polymer Property : Shear Strength = 21.226 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.14635 MPa

@Shear Rate 500 1/s,
Temperature 270 °C
21.226 psi

@Shear Rate 500 1/s,
Temperature 518 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high ..