Material Notes:
Zytel® 7331J NC010 is lubricated fast cycling PA6 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa

@Temperature 23.0 °C
11600 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 40 %

@Temperature 23.0 °C
40 %

@Temperature 73.4 °F
50mm/min; DAM; ISO 527
Elongation at Yield 4.0 %

@Temperature 23.0 °C
4.0 %

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 2.90 GPa

@Temperature 23.0 °C
421 ksi

@Temperature 73.4 °F
DAM; ISO 527
Flexural Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
DAM; ISO 178
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
DAM; ISO 75-1/-2
Flammability, UL94 V-2

@Thickness 6.00 mm
V-2

@Thickness 0.236 in
DAM; IEC 60695-11-10
V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
DAM; IEC 60695-11-10
V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
DAM; IEC 60695-11-10
V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
DAM; IEC 60695-11-10
V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
DAM; UL94
V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
DAM; UL94
V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
DAM; UL94
V-2

@Thickness 6.00 mm
V-2

@Thickness 0.236 in
DAM; UL94
Processing Properties Metric English Comments
Melt Temperature 260 - 280 °C
500 - 536 °F
DAM
Mold Temperature 50.0 - 90.0 °C
122 - 194 °F
DAM
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Forms Pellets
DAM
Generic Nylon 6
DAM
Material Status Preliminary Data
DAM
Part Marking Code >PA6<
ISO 11469; DAM
Processing Method Injection Molding
DAM
Product Category Unreinforced Resins
DAM
Resin Identification PA6
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM
Users viewing this material also viewed the following: