Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 4Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cm
0.017 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 41
41
15s; ISO 868
<= 44
<= 44
ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527-1/-2
Tensile Stress 8.40 MPa

@Strain 10.0 %
1220 psi

@Strain 10.0 %
ISO 527-1/-2
14.0 MPa

@Strain 50.0 %
2030 psi

@Strain 50.0 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
350 %
350 %
Nominal; ISO 527-1/-2
Tensile Modulus 0.100 GPa
14.5 ksi
ISO 527-1/-2
Flexural Modulus 0.100 GPa
14.5 ksi
ISO 178
Charpy Impact, Notched NB
NB
ISO 179/1eA
Tear Strength 109 kN/m
622 pli
normal; ISO 34-1
112 kN/m
639 pli
parallel; ISO 34-1
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 210 µm/m-°C
117 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 200 µm/m-°C
111 µin/in-°F
ISO 11359-1/-2
Melting Point 206 °C
403 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Part Marking Code >TPC-ET<
ISO 11469
Processing Blow Moulding
Profile Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification TPC-ET
ISO 1043
Special Characteristics Heat stabilised or stable to heat