Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 109 kN/m | 622 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible XV3683 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 109 kN/m | 620 pli | Die C |
Elastomer Engineering E50D Polyurethane A polyester-based urethane with excellent strength, resilience, and abrasion resistance. Excellent in heavy-duty applications and where oils and solvents are present. Information provided by Elasto.. |
|||
Tear Strength | 109 kN/m | 622 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |
|||
Tear Strength | 109 kN/m | 620 pli | ASTM D624 |
Dow SPECTRIM™ 50-S Reaction Moldable Polymer SPECTRIM™ 50-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p.. |