Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.100 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.100 GPa
14.5 ksi
ISO 178
Polimeri Europa Greenflex® ML 20 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 20 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required.Main Applications: Greenflex ML 20 is recommended for the production of flexible ite..
Flexural Modulus 0.100 GPa
14.5 ksi
ISO 178
Polimeri Europa Greenflex® ML 21 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 21 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required. Greenflex ML 21 contains additive waxes to obtain high production speed.Main Applic..
Flexural Modulus 0.100 GPa
14.5 ksi
ISO 178
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding
Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa.
Flexural Modulus 0.100 GPa

@Temperature 23.0 °C
14.5 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET  (Unverified Data**)
Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,..
Flexural Modulus 0.100 GPa
14.5 ksi
ASTM D790
Rotuba M Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Flexural Modulus 0.100 GPa
14.5 ksi
1% Secant; ASTM D790
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
Flexural Modulus 0.100 GPa
14.5 ksi
1% secant at 0.05 in/min; ASTM D790A
LyondellBasell Astryn CA743GA Polypropylene Copolymer
Key Features: low melt flow, low modulus, UV-stabilized polypropylene copolymer with antiblock, good heat seamability, good puncture resistance, plasticizer-free, excellent low temperature impact re..
Flexural Modulus 0.100 GPa
14.5 ksi
Tangent, 0.5 in/min; ASTM D790
LyondellBasell Hifaxâ„¢ CA10GC Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA10GC fractional melt flow, 100 MPa flexural modulus, precolored, UV-stabilized, reactor grade, extrudable thermoplastic elastomeric olefin (TEO) resin combines good proces..
Flexural Modulus 0.100 GPa
14.5 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCA871A PPE
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
Flexural Modulus 0.100 GPa
14.5 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCA871A PPE
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
Flexural Modulus 0.100 GPa
14.5 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCA871A PPE (Asia Pacific)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
Flexural Modulus 0.100 GPa
14.5 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCA871A PPE (Asia Pacific)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
Flexural Modulus 0.100 GPa
14.5 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCA871A PPE (Europe-Africa-Middle East)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
Flexural Modulus 0.100 GPa
14.5 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCA871A PPE (Europe-Africa-Middle East)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
Flexural Modulus 0.100 GPa
14.5 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD915 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation materials. Flame retardant performance capable of meeting UL 1581 VW-1 require..
Flexural Modulus 0.100 GPa
14.5 ksi
ASTM D790
Borealis Casico™ FR4807 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Casico FR4807 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4804 offers a unique combination of good extrusion pr..
Flexural Modulus 0.100 GPa
14.5 ksi
ASTM D790
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium
Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Flexural Modulus 0.100 GPa
14.5 ksi
ASTM D790
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
Flexural Modulus 0.100 GPa
14.5 ksi
ISO 178
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi..
Flexural Modulus 0.100 GPa
14.5 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR4525 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Flexural Modulus 0.100 GPa
14.5 ksi
ASTM D790
Buckeye Polymers BP Flex D0840 TPO
Replace Flex PVCTPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resis..
Flexural Modulus 0.100 GPa
14.5 ksi
ASTM D790
Ashley Polymers Ashlene® R6020 Nylon 6
A medium viscosity extrusion grade resin with excellent melt stability and good melt strength, suitable for extrusion coating and film co-extrusion applications. Excellent grease resistance, toughn..
Flexural Modulus 0.100 - 9.50 GPa
14.5 - 1380 ksi
Average value: 2.15 GPa Grade Count:327
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Copyright © lookpolymers.com All Rights Reserved