Mechanical Properties Metric English Comments
Tensile Stress 8.40 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1220 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET  (Unverified Data**)
Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,..
Tensile Stress 8.40 MPa

@Strain 100 %
1220 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® PL381-H TPC-ET
Injection Molding
Tensile Stress 8.40 MPa

@Strain 10.0 %
1220 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® PM460-H TPC-ET
Injection Molding, Heat Stabilized
Tensile Stress 8.40 MPa

@Strain 50.0 %
1220 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.40 MPa

@Strain 47.19 %,
Temperature 120 °C
1220 psi

@Strain 47.19 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.40 MPa

@Strain 5.68 %,
Time 36000 sec
1220 psi

@Strain 5.68 %,
Time 10.0 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Strain 6.81 %,
Time 3.60e+6 sec
1220 psi

@Strain 6.81 %,
Time 1000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Time 3600 sec,
Strain 4.98 %
1220 psi

@Time 1.00 hour,
Strain 4.98 %
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Strain 6.32 %,
Time 360000 sec
1220 psi

@Strain 6.32 %,
Time 100 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Strain 7.26 %,
Time 3.60e+7 sec
1220 psi

@Strain 7.26 %,
Time 10000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.40 MPa

@Strain 0.0400 %,
Temperature 40.0 °C
1220 psi

@Strain 0.0400 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..
Tensile Stress 8.40 MPa

@Strain 50.0 %
1220 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers
Tensile Stress 8.40 MPa

@Strain 10.0 %
1220 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi..