Akzo Nobel Blow Molding of HDPE with 3.25 % Expancel

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Akzo Nobel, Expancel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Blow Molding of HDPE with 3.25 % Expancel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.760 g/cc
0.0275 lb/in³
blow pressure of 2 Bar; 20% density reduction