PolyOne Edgetek® MLS-10GF/000 Polysulfone Alloy - 10% Glass Fiber Reinforced  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® MLS-10GF/000 Polysulfone Alloy - 10% Glass Fiber Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Water Absorption 0.18 %

@Thickness 3.17 mm
0.18 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 86.2 MPa
12500 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 3.0 - 4.0 %
3.0 - 4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 4.62 GPa
670 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 332 - 349 °C
630 - 660 °F
Molding