Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 109 kN/m | 622 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible XV3683 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 109 kN/m | 622 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |