Material Notes:
15% Glass Reinforced, Flame Retardant, Injection Molding, High Flow
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
dry; ISO 1183
Moisture Absorption 2.00 %
2.00 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 122 MPa
17700 psi
dry; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
dry; ISO 527-1/-2
Flexural Strength 135 MPa
19600 psi
cond; ISO 178
180 MPa
26100 psi
dry; ISO 178
Flexural Modulus 4.20 GPa
609 ksi
cond; ISO 178
6.00 GPa
870 ksi
dry; ISO 178
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
dry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
dry; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
dry; IEC 60695-11-10